Carima
Carima Dent-Castable Wax
Castable
Direct casting for dental alloy crowns, jewelry casting; Carima DM400 & IM-D
Full specifications
Mechanical
- Tensile strength
- 19 MPa
- Elongation at break
- 5 %
- Flexural strength
- 28 MPa
- Flexural modulus
- 680 MPa
- Shore hardness
- 72D
- Compressive strength
- 35 MPa
Thermal
- HDT @ 0.45 MPa
- 46 °C
- HDT @ 1.82 MPa
- 35 °C
- Glass transition
- 45 °C
- Max service temp
- 38 °C
Curing & print
- Viscosity @ 25°C
- 195 cP
- Cure wavelength
- 405nm nm
- Post-cure
- Direct burnout without post-cure
- Shrinkage / accuracy
- 1.20%
- Water-washable
- No
Physical
- Density
- 1.11 g/cm³
- Available colors
- Red / Green
- Biocompatibility
- Clean ash-free burnout